| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
|
RheTech Products FT4700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
|
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
|
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral
Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
|
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
|
RheTech Products T10P102-00EG 10% Talc Reinforced Polypropylene, Extrusion Grade, Natural
Injection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
|
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural
Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
|
RheTech Products T10P250-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black
Applications: Wire troughFan shroudsElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 210 - 221 °C | 410 - 430 °F | |
|
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated
Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
|
Ravago Manufacturing Americas Hylac® HF96 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
|
|||
| Nozzle Temperature | 210 - 241 °C | 410 - 465 °F | |
|
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
|
|||
| Nozzle Temperature | 210 - 220 °C | 410 - 428 °F | Injection Molding |
|
LG Chemical LI911 ASA
Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
|
LG Chemical LUMILOY GN1006F Injection Molding FR mPPO
Uses include electric/electronic parts.
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical LUPOL ED1045D TPO, Thermoplastic Elastomer
Description: Injection Molding, TPO, Thermoplastic Elastomer, Soft TouchApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 1333-86-4, 25087-34-7 and 14807-96-6Information provided..
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical LUPOL HI4352L PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9003-07-0, 26221-73-8 and 14807-96-6Inform..
|
|||
| Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
|
LG Chemical LUPOL TE-5202U Thermoplastic Elastomer Alloy, 20% Polymer Alloy, High Impact, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical MP220 ABS, High Adhesion, Heat Resistance
Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical
|
|||
| Nozzle Temperature | 210 °C | 410 °F | |
|
Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane
Type : Pearlthane® D91T80 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties...
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical LUPOL GP3102Y PP+MF10%, High Impact, High Flow
Description: Injection Molding, PP+MF10%, General Purpose, High Impact, High FlowApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemica..
|
|||
| Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
|
LG Chemical LUPOL HF-3308 High Flow Polypropylene, 30% Mineral Fillers
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical LUPOL HF5150H PP+MF15%, High Flow
Description: Injection Molding, PP+MF15%, High FlowApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical LUPOL HM3207 PP+MF20%, High Stiffness
Description: Injection Molding, PP+MF20%, Good Weatherability, High StiffnessApplication: Automotive Interior Parts CAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
|
|||
| Nozzle Temperature | 210 - 240 °C | 410 - 464 °F | |
|
LG Chemical LUPOL HM-4354 Heat Resistant Polypropylene, 35% Glass Fiber/Mineral Filler Reinforced, High Strength, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical LUPOL LW4302 PP+GF/MF30%
Description: Injection Molding, PP+GF/MF30%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 14807-96-6 and 165997-17-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
|
LG Chemical LUPOL TE5104 PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
|
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets
LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron..
|
|||
| Nozzle Temperature | 210 °C | 410 °F | |
|
Lubrizol Advanced Materials PEARLTHANE® D11H95S Thermoplastic Polyurethane Elastomer
PEARLTHANE® D11H95S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out..
|
|||
| Nozzle Temperature | 210 °C | 410 °F | |
|
Lubrizol Advanced Materials Pearlthane® D16N60D Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 16N60D is a polyether-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining high hardness with excellent mechanical properties and ..
|
|||
| Nozzle Temperature | 210 °C | 410 °F | Typical Die Temp. |
|
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res..
|
|||
| Nozzle Temperature | 210 - 230 °C | 410 - 446 °F | |
|
Tisan TISLAMID® 6 UNR Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Nozzle Temperature | 210 - 238 °C | 410 - 460 °F | |
|
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||