Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Rear Barrel Temperature = 190 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Huntsman AVALON® 60 DB Thermoplastic Polyurethane
Introduction: AVALON 60 DB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DB is part of the AVALON Perform Range and offers a premium soling materi..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Huntsman AVALON® 60 DE Thermoplastic Polyurethane
Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical KEYFLEX BT 1047D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
LG Chemical KEYFLEX TO-1045D Thermoplastic Olefin for Injection Molding, 45D Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Rear Barrel Temperature 190 - 220 °C
374 - 428 °F
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical LUPOL ED1045D TPO, Thermoplastic Elastomer
Description: Injection Molding, TPO, Thermoplastic Elastomer, Soft TouchApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 1333-86-4, 25087-34-7 and 14807-96-6Information provided..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical LUPOL GP3202Z PP+MF20%
Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss
Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical LUPOL HI5204 PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical LUPOL HI5302A PP+MF15%, High Impact
Description: Injection Molding, PP+MF15%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical LUPOL HI5302RB PP+MF25%, High Impact
Description: Injection Molding, PP+MF25%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical LUPOL TE5208 PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
Rear Barrel Temperature 190 - 260 °C
374 - 500 °F
Injection
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet..
Rear Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Inno-Comp INNOPOL® CS 2-2523 EP 16% Talc Filled, Elastomer Modified Polypropylene Copolymer
INNOPOL® CS 2-2523 EP is a 16% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in natural and custom colored form.INNOPOL® CS 2-2523 EP..
Rear Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Inno-Comp INNOPOL® CS 2-3840 MO 40% Glass Filled Polypropylene Copolymer
INNOPOL® CS 2-3840 MO is a 40 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-3840 MO is recommended for p..
Rear Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Inno-Comp INNOPOL® CS 2-5830 SA 30% Glass Filled Polypropylene Copolymer
INNOPOL® CS 2-5830 SA is a 30 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-5830 SA is recommended for p..
Rear Barrel Temperature 190 - 200 °C
374 - 392 °F
Huntsman AVALON® 80 AB Thermoplastic Polyurethane
Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma..
Rear Barrel Temperature 190 - 200 °C
374 - 392 °F
Huntsman AVALON® 85 AB Thermoplastic Polyurethane
Introduction: AVALON 85 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 AB is part of the AVALON Performance Range and offers a premium soling ma..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane
Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling ..
Rear Barrel Temperature 190 - 200 °C
374 - 392 °F
Huntsman AVALON® 92 AB Thermoplastic Polyurethane
Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical LUPOL GP3400S PP+MF40%
Description: Injection Molding, PP+MF40%, General Purpose, Low WarpageApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 12001-26-2Information provided by LG Chemica..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
LG Chemical LUPOS GP-2200H General Purpose ABS, 20% Glass Fiber Reinforced, High Heat Resistance
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Aft-1. Region Temperature
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Aft-1. Region Temperature
Tisan TISOPLEN® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Rear Barrel Temperature 190 - 210 °C
374 - 410 °F
Aft-1. Region Temperature
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Rear Barrel Temperature 190 °C
374 °F
Injection
Alliance Polymers Viprene™ G45D-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G45D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Rear Barrel Temperature 190 °C
374 °F
Beijing Chemical Industry KAIFA® GL5200 ABS Extrusion Grade
Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group)
Rear Barrel Temperature 190 °C
374 °F
Beijing Chemical Industry KAIFA® GL5100 ABS Extrusion Grade
Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group)
Rear Barrel Temperature 190 - 200 °C
374 - 392 °F
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane
Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi..
Copyright © lookpolymers.com All Rights Reserved