| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
|
PolyOne OnFlex™ BIO 5180D-E0014 Thermoplastic Elastomer (TPE)
OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
|
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE)
OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | |
|
Oxford Polymers PP-Homopolymer-20GF-Natural PP, 20% Glass Fiber Reinforced
Product Description: Glass Fiber (20% Reinforced), Polypropylene injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Improved stiffnessInfor..
|
|||
| Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
|
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
|
|||
| Dry Time |
1.00
hour @Temperature 20.0 °C |
1.00
hour @Temperature 68.0 °F |
|
|
Guarniflon TENFIL TF 200 Polytetrafluoroethylene Thread Sealant
TENFIL TF200 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti..
|
|||
| Dry Time |
1.00
hour @Temperature 20.0 °C |
1.00
hour @Temperature 68.0 °F |
|
|
Guarniflon TENFIL TF 400 Polytetrafluoroethylene Thread Sealant
TENFIL TF400 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti..
|
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4040-S High Temperature Protective Coating Silicone-Polyester |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled
CP5000 is a two part, water-based, inorganic zinc rich primer which provides superior resistance to salt-fog, immersion, impact and abrasion. This primer system is compatible with all CP-Series prod..
|
|||
| Dry Time | 1.00 - 2.00 hour | 1.00 - 2.00 hour | Touch |
|
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
|
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
|
|||
| Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
|
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
|
|||
| Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
|
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou..
|
|||
| Dry Time | 1.00 - 3.00 hour | 1.00 - 3.00 hour | |
|
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded
Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo..
|
|||