| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
|
Unitika AX-1500W Conditioned
Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis..
|
|||
| Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
|
Unitika AXF-1500-05 Conditioned
Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd.
|
|||
| Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
|
Unitika AXF-1500-05 Dry
Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd.
|
|||
| Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
|
Unitika LM-8503-10
Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd.
|
|||
| Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
|
Unitika P-1001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
|
|||
| Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
|
Unitika P-5001 Engineering Plastic
P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra..
|
|||
| Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
|
Unitika UG-100-20 Engineering Plastic
Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd.
|
|||
| Dry Time | 8.00 - 24.0 hour | 8.00 - 24.0 hour | |
|
Unitika FUN-8000
Characteristics: High impact strength High chemical resistance Transparency as high as polycarbonateInformation provided by Unitika Ltd.
|
|||
| Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
|
Unitika U-100 Engineering Plastic
CAS No: 26590-50-1Information provided by Unitika Ltd.
|
|||
| Dry Time | 6.00 - 24.0 hour | 6.00 - 24.0 hour | |
|
Unitika UG-100-30 Engineering Plastic
Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd.
|
|||
| Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
|
Unitika UM-8430RG
Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd.
|
|||
| Dry Time | 2 - 24.0 hour | 2 - 24.0 hour | |
|
Chi Mei Polylac® PA-747 ABS
High impact
|
|||
| Dry Time | 2 - 24.0 hour | 2 - 24.0 hour | |
|
Chi Mei Polylac® PA-765 ABS - Flame Retardant
F.R. High Flow
|
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4010S High Temperature Protective Coating Silicone-Polyester |
|||
| Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled
Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C).
|
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
| Dry Time | 1.0 - 24.0 hour | 1.0 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Dry Time | 1.00 - 24.0 hour | 1.00 - 24.0 hour | Recoat |
|
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
| Dry Time | 10.0 - 24.0 hour | 10.0 - 24.0 hour | |
|
Unitika U-8000
U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than..
|
|||