| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness 0.800 mm
|
7.0
-
15
sec <br>@Thickness 0.0315 in
|
UL 746 |
|
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated
General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness 0.851 mm
|
7.0
-
15
sec <br>@Thickness 0.0335 in
|
UL 746 |
|
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical HG173 ABS, High Surface Gloss
Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical HI100K ABS, High Impact
Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical HIPS MI770 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=0.710 mm
|
7.0
-
15
sec <br>@Thickness >=0.0280 in
|
|
|
LG Chemical LUCEL N127LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical LUCEL N127LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical Lupox® GP1000S PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical Lupox® GP2100 PBT+GF10%
Description: Injection Molding, PBT+GF10%, General Purpose Application: IT/OA, E&E, Automotive (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=3.00 mm
|
7.0
-
15
sec <br>@Thickness >=0.118 in
|
|
|
LG Chemical Lupox® GP2400G PBT+GF40%
Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance
Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical XR409E ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical XR401T ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.710 mm
|
7.0
-
14
sec <br>@Thickness 0.0280 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.400 mm
|
7.0
-
14
sec <br>@Thickness 0.0157 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 1.50 mm
|
7.0
-
14
sec <br>@Thickness 0.0591 in
|
UL 746A |
|
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.400 mm
|
7.0
-
14
sec <br>@Thickness 0.0157 in
|
UL 746A |
|
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness 0.750 mm
|
7.0
-
15
sec <br>@Thickness 0.0295 in
|
UL 746A |
|
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded
Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent ..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness 1.50 mm
|
7.0
-
15
sec <br>@Thickness 0.0591 in
|
UL 746A |
|
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded
Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent ..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 3.00 mm
|
7.0
-
14
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM
Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 3.00 mm
|
7.0
-
14
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 1.50 mm
|
7.0
-
14
sec <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 3.00 mm
|
7.0
-
14
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness 3.00 mm
|
7.0
-
15
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 1.50 mm
|
7.0
-
14
sec <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.710 mm
|
7.0
-
14
sec <br>@Thickness 0.0280 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM
Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness 0.710 mm
|
7.0
-
15
sec <br>@Thickness 0.0280 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded
Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold ..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 3.00 mm
|
7.0
-
14
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||