| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded |
| Manufacturer | LG Chemical |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical XR409E ABS, Heat Resistance.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.010 | 0.010 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 5.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 111 | 111 | ASTM D785 |
| Tensile Strength, Yield | 48.1 MPa @Thickness 3.20 mm |
6970 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
| Elongation at Break | 20 % @Thickness 3.20 mm |
20 % @Thickness 0.126 in |
50 mm/min; ASTM D638 |
| Flexural Yield Strength | 76.5 MPa @Thickness 3.20 mm |
11100 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
| Flexural Modulus | 2.45 GPa @Thickness 3.20 mm |
356 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
| Izod Impact, Notched | 1.57 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.94 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| 1.67 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.12 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 | |
| Izod Impact, Unnotched | 0.785 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
1.47 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
| 0.785 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 112 °C @Thickness 6.40 mm |
234 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 104 °C @Thickness 6.40 mm |
219 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Vicat Softening Point | 114 °C @Load 5.00 kg |
237 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
| UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
| 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B | |
| UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
| 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B | |
| UL RTI, Mechanical without Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
| 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B | |
| Flammability, UL94 | HB @Thickness >=1.50 mm |
HB @Thickness >=0.0591 in |
|
| HB @Thickness >=3.00 mm |
HB @Thickness >=0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Dielectric Strength | 33.0 kV/mm @Thickness 1.00 mm |
838 kV/in @Thickness 0.0394 in |
ASTM D149 |
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | ASTM D495 |
| Comparative Tracking Index | >= 600 V | >= 600 V | Solution A; IEC 60112 |
| Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
| 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
||
| High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
| >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
||
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 180 - 220 °C | 356 - 428 °F | Injection Molding |
| Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
| Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
| Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
| Melt Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Injection Molding |
| Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Injection Molding |
| Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour | Injection Molding |
| Back Pressure | 1.96 - 3.92 MPa | 284 - 569 psi | Injection Molding |
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm | Injection Molding |