| Category | Polymer , Thermoplastic , Polyetherimide (PEI) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | ULTEM |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics ULTEM 9076 PEI (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.30 g/cc | 0.0470 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.700 % | 0.700 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 1.25 % | 1.25 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | on Tensile Bar; SABIC Method |
| Melt Index of Compound | 22 g/10 min @Load 5.00 kg, Temperature 360 °C |
22 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, H358/30 | 145 MPa | 21000 psi | ISO 2039-1 |
| Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
| Tensile Strength, Yield | 95.0 MPa | 13800 psi | 50 mm/min; ISO 527 |
| Elongation at Break | 50 % | 50 % | 50 mm/min; ISO 527 |
| Elongation at Yield | 6.0 % | 6.0 % | 50 mm/min; ISO 527 |
| Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 135 MPa | 19600 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 3.00 GPa | 435 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
| 6.00 kJ/m² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| 0.600 J/cm² @Temperature -30.0 °C |
2.86 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
| Thermal Conductivity | 0.260 W/m-K | 1.80 BTU-in/hr-ft²-°F | ISO 8302 |
| Deflection Temperature at 0.46 MPa (66 psi) | 195 °C | 383 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 175 °C | 347 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 200 °C | 392 °F | Rate B/50; ISO 306 |
| 200 °C | 392 °F | Rate B/120; ISO 306 | |
| 210 °C | 410 °F | Rate A/50; ISO 306 | |
| Oxygen Index | 50 % | 50 % | ISO 4589 |
| Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ROA; IEC 60093 |
| Dielectric Constant | 2.8 @Frequency 1.00e+6 Hz |
2.8 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 2.9 @Frequency 50.0 - 60.0 Hz |
2.9 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| Dielectric Strength | 18.0 kV/mm @Thickness 3.20 mm |
457 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
| Dissipation Factor | 0.0050 @Frequency 1.00e+6 Hz |
0.0050 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 150 V | 150 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |