| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group 2557 AMC Polyester
Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low ..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group 2567 AMC
Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and ..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group 5553 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group 6502 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound
Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on ..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group RALUPOL® 4385 UP
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group RALUPOL® 4806 UP
Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Techmer ES HiFill® PA6 0500
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Techmer ES HiFill® PA6 0685
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 105E3V36327 Acetate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp
Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 285E3720005 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 307A4000015 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 307E0V16310 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 307E4000018 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 350A4861313 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp
Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 360A4861316 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 360E461312 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp
Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp
Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp
Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp
Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl..
|
|||
| Volume Resistivity | 1.00e+14 - 1.00e+15 ohm-cm | 1.00e+14 - 1.00e+15 ohm-cm | IEC 60093 |
|
Raschig Group RALUPOL® 8605 UP Polyester
Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire..
|
|||
| Volume Resistivity | 1.00e+13 - 1.00e+15 ohm-cm | 1.00e+13 - 1.00e+15 ohm-cm | ASTM D257 |
|
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp
(discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
|
|||