Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Tenite 285E3720005 Butyrate Clear, Trsp

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Cellulose Acetate Butyrate, Molded
Manufacturer Eastman Chemical
Trade Name Tenite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Tenite 285E3720005 Butyrate Clear, Trsp.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers, or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulose Acetate Butyrate 285-05 contains an odor mask and has a plasticizer level of 5%.Applications/UsesAppliancesConsumer-personal careProfiles
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 1.6 %
1.6 %
24h Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Collected Volatile Condensable Material 0.25 %
0.25 %
Weight loss on heating, 72hrs, 80°C; ASTM D707
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength at Break 51.0 MPa
7400 psi
ASTM D638
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D638
Flexural Yield Strength 57.2 MPa
8300 psi
ASTM D790
Flexural Modulus 1.724 GPa
250.0 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm

@Temperature -40.0 °C
1.59 ft-lb/in

@Temperature -40.0 °F
ASTM D256
1.65 J/cm

@Temperature 23.0 °C
3.09 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 110 - 170 µm/m-°C

@Temperature 20.0 °C
61.1 - 94.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.26 - 1.67 J/g-°C
0.301 - 0.399 BTU/lb-°F
DSC
Thermal Conductivity 0.170 - 0.330 W/m-K
1.18 - 2.29 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
ASTM D648
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.46 - 1.49
1.46 - 1.49
n<sub>D</sub>; ASTM D542
Haze <= 8.5 %
<= 8.5 %
ASTM D1003
Transmission, Visible >= 90 %

@Thickness 1.52 mm
>= 90 %

@Thickness 0.0598 in
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 - 1.00e+15 ohm-cm
1.00e+13 - 1.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.3 - 3.8

@Frequency 1e+6 Hz
3.3 - 3.8

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.8 - 18.7 kV/mm
300 - 475 kV/in
ASTM D149
Dissipation Factor 0.010 - 0.15

@Frequency 1e+6 Hz
0.010 - 0.15

@Frequency 1e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Plasticizer, % 5
Soluble Matter Loss, % 0.1
ASTM D570