| Greene Tweed Arlon® 1000 Polyketone |
Polyetheretherketone (PEEK) |
Arlon®
|
| Greene Tweed Arlon® 1160 PEEK, Glass Filled |
Polyetheretherketone, PEEK, Glass Fiber Filled |
Arlon®
|
| Greene Tweed Arlon® 1163 PEEK, Glass Filled |
Polyetheretherketone, PEEK, Glass Fiber Filled |
Arlon®
|
| Greene Tweed Arlon® 1260 Polyketone, Carbon Filled |
Polyetheretherketone (PEEK) |
Arlon®
|
| Greene Tweed Arlon® 1286 Polyketone, Carbon Filled |
Polyetheretherketone (PEEK) |
Arlon®
|
| Greene Tweed Arlon® 1330 PEEK |
Polyetheretherketone, PEEK, Unreinforced |
Arlon®
|
| Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled |
Polyetheretherketone, PEEK, Carbon Fiber Filled |
Arlon®
|
| Greene Tweed Arlon® 2000 Polyketone |
Polyetheretherketone (PEEK) |
Arlon®
|
| Greene Tweed ARâ„¢ 1 Abrasive-Resistant Thermoplastic |
Thermoplastic |
AR™
|
| Greene Tweed ARâ„¢ HT Abrasive-Resistant Thermoplastic |
Thermoplastic |
AR™
|
| Greene Tweed Avalon® 1 PTFE |
Polytetrafluoroethylene (PTFE), Molded |
Avalon®
|
| Greene Tweed Avalon® 11 PTFE, Carbon, Graphite Filled |
Polytetrafluoroethylene (PTFE), Carbon Fiber Filled |
Avalon®
|
| Greene Tweed Avalon® 16 PTFE, Glass, Molybdenum Filled |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
Avalon®
|
| Greene Tweed Avalon® 56 PTFE |
Polytetrafluoroethylene (PTFE), Molded |
Avalon®
|
| Greene Tweed Avalon® 57 PTFE, Thermoset Resin Filled |
PTFE |
Avalon®
|
| Greene Tweed Avalon® 69 PTFE, Thermoplastic and Carbon Filled |
Polytetrafluoroethylene (PTFE), Carbon Fiber Filled |
Avalon®
|
| Greene Tweed Avalon® 7 PTFE, Pigmented and Molybdenum Filled |
PTFE |
Avalon®
|
| Greene Tweed Avalon® 87 PTFE, Glass Filled |
Polytetrafluoroethylene (PTFE), Glass Filled, Molded |
Avalon®
|
| Greene Tweed Avalon® 89 PTFE |
PTFE |
Avalon®
|
| Greene Tweed Avalon® 9 PTFE, Graphite Filled |
Polytetrafluoroethylene (PTFE), Conductive Carbon Filled |
Avalon®
|
| Greene Tweed CHEMRAZ® 504 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 505 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 510 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 513 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 514 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 517 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 522 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 526 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 528 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 534 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 537 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 543 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 555 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 565 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 571 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 584 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 585 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 592 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 605 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 615 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 618 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 644 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 655 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® E38 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® SD585 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® SD625 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed FLUORAZ® 784 Fluoroelastomer, FEPM |
Thermoset Fluoroelastomer |
FLUORAZ®
|
| Greene Tweed FLUORAZ® 790 Fluoroelastomer, FEPM |
Thermoset Fluoroelastomer |
FLUORAZ®
|
| Greene Tweed FLUORAZ® 799 Fluoroelastomer, FEPM |
Thermoset Fluoroelastomer |
FLUORAZ®
|
| Greene Tweed FLUORAZ® 888 Fluoroelastomer, FEPM |
Thermoset Fluoroelastomer |
FLUORAZ®
|
| Greene Tweed Fluoroelastomer 742 FKM |
Thermoset Fluoroelastomer |
Fluoroelastomer
|
| Greene Tweed Fluoroelastomer 931 FKM |
Thermoset Fluoroelastomer |
Fluoroelastomer
|
| Greene Tweed FPD Blueâ„¢ 707 Fluoroelastomer |
Thermoset Fluoroelastomer |
FPD Blue™
|
| Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber |
Polyetheretherketone, PEEK, Carbon Fiber Filled |
Orthetek®
|
| Greene Tweed WRâ„¢ 300 PEEK, Carbon Filled |
Polyetheretherketone, PEEK, Carbon Fiber Filled |
WR™
|
| Greene Tweed WRâ„¢ 525 PEEK, Carbon Filled |
Polyetheretherketone, PEEK, Carbon Fiber Filled |
WR™
|
| Greene Tweed WRâ„¢ FP100 Polyketone, Reinforced |
Polyetheretherketone (PEEK) |
WR™
|
| Greene Tweed Xycomp® 1001-01 PEEK, Carbon Fiber Filled |
Polyetheretherketone, PEEK, Carbon Fiber Filled |
Xycomp®
|
| Greene Tweed Xycomp® 1030-01 Carbon/Nylon 12 Composite |
Nylon 12 |
Xycomp®
|
| Greene Tweed Xycomp® 1030-02 Carbon/Nylon 12 Composite |
Nylon 12 |
Xycomp®
|
| Greene Tweed Xyfluor® 860 Fluorinated Elastomer Compound |
Thermoset Fluoroelastomer |
Xyfluor®
|
| Greene Tweed Arlon® 1263 PEEK, Carbon Filled |
Polyetheretherketone, PEEK, Carbon Fiber Filled |
Arlon®
|
| Greene Tweed Avalon® 44 PTFE, Mineral, Molybdenum Filled |
Polytetrafluoroethylene (PTFE), Mica Filled |
Avalon®
|
| Greene Tweed CHEMRAZ® 520 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 550 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 551 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 570 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 600 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 629 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 639 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 640 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 653 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 656 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed CHEMRAZ® 661 Perfluoroelastomer |
Thermoset Fluoroelastomer |
CHEMRAZ®
|
| Greene Tweed FLUORAZ® 797 Fluoroelastomer, FEPM |
Thermoset Fluoroelastomer |
FLUORAZ®
|
| Greene Tweed FLUORAZ® 890 Fluoroelastomer, FEPM |
Thermoset Fluoroelastomer |
FLUORAZ®
|
| Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber |
Polyetheretherketone, PEEK, Carbon Fiber Filled |
Orthetek®
|
| Greene Tweed WRâ„¢ 575 PEEK, Bi-Directional Carbon Fiber Filled |
Polyetheretherketone, PEEK, Carbon Fiber Filled |
WR™
|
| Greene Tweed Xyfluor® 870 Fluorinated Elastomer Compound |
Thermoset Fluoroelastomer |
Xyfluor®
|