Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Greene Tweed CHEMRAZ® 510 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® 510 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Greene Tweed’s Chemraz® 510, a perfluoroelastomer, offers an extremely broad range of chemical resistance with a Shore A hardness value of 90. with a temperature range form -22°F to 446°F (-30°C to 230°C), Chemraz 510 is well suited for use in a range of applications, from mechanical seals to pump housings.Because of its versatility, Chemraz 510 is often used as a standard compound for sealing at high pressures. It can be found in a variety of fluids and solutions including acids, caustics, aldehydes, esters, aromatics, hot water, steam, amines, methanol, ketones, TBA and many other custom shapes.Applications: Mechanical sealsValvesPump HousingsSampling/metering equipmentCompressorsReactorsMixersControls/instrumentationSprayers/dispensersCouplingsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength at Break 13.62 MPa
1975 psi
ASTM D1414
Tensile Strength, Yield 7.58 MPa
1100 psi
@ 50% Elongation; ASTM D1414
Elongation at Break 85 %
85 %
ASTM D1414
Compression Set 30 %
30 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: