3M Dyneon™ TFM™ 1700 PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer 3M Dyneon™
Trade Name TFM™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TFM™ 1700 PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Meets ASTM D4894 Type III, Grade 1 resinNon-free-flowing compression molding powderVery fine particle sizeDense polymer structure, low permeabilityImproved weldabilityLow deformation under loadGood electrical and mechanical propertiesIncreased modulus of elasticityLow molding pressureExcellent for production of very thin films with superior permeation propertiesInformation provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.16 g/cc
2.16 g/cc
@ 23°C, Sintering Molding; ASTM D4894-98a
Bulk Density 0.420 g/cc
0.0152 lb/in³
ASTM D4894-98a
Particle Size 25 µm
25 µm
average; ASTM D4894-98a
Deformation 4.0 %
4.0 %
2175 psi - permanent, 23°C, Sintering Molding; ASTM D621
8.0 %
8.0 %
2175 psi - 24 hrs, 23°C, Sintering Molding; ASTM D621
9.0 %
9.0 %
2175 psi - 100 hrs, 23°C, Sintering Molding; ASTM D621
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.1 MPa
4800 psi
Sintered Molding; ASTM D4894-98a
Elongation at Break 450 %
450 %
Sintered Molding; ASTM D4894-98a
Tensile Modulus 0.6498 GPa
94.25 ksi
Sintered Molding; ASTM D638
Thermal Properties Metric English Comments
Melting Point 317 - 337 °C
603 - 639 °F
second; ASTM D4894-98a
332 - 352 °C
630 - 666 °F
initial; ASTM D4894-98a
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-330 °F
Flammability, UL94 V-0
V-0
Shrinkage 5.80 %

@Temperature 23.0 °C
5.80 %

@Temperature 73.4 °F
Sintering Moldings; ASTM D4894-98a
Electrical Properties Metric English Comments
Dielectric Strength 146 kV/mm
3710 kV/in
ASTM D149-95a