| Category | Ceramic , Oxide , Aluminum Oxide |
| Manufacturer | 3M |
| Trade Name | Nextel™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | 3M Nextel™ AF-30 Industrial Woven Fabric 312.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.70 g/cc | 0.0975 lb/in³ | |
| Permeability | 50 | 50 | [ft<sup>3</sup>/min/ft<sup>2</sup>], Air w/o sizing |
| Thickness | 760 microns | 29.9 mil | |
| Fiber Count | 2000 dtex | 1800 denier | 1/2 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 1700 MPa | 247000 psi | filament 25.4mm |
| Tensile Modulus | 152 GPa | 22000 ksi | filament |
| Tear Strength | 31.4 kN/m | 179 pli | Fill, Breaking Strength w/o Sizing |
| 388 kN/m | 2220 pli | Warp, Breaking Strength w/o Sizing |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 3.00 µm/m-°C @Temperature 25.0 - 500 °C |
1.67 µin/in-°F @Temperature 77.0 - 932 °F |
|
| Specific Heat Capacity | 1.05 J/g-°C @Temperature 500 °C |
0.251 BTU/lb-°F @Temperature 932 °F |
|
| Thermal Conductivity | 0.105 W/m-K @Temperature 93.0 °C |
0.729 BTU-in/hr-ft²-°F @Temperature 199 °F |
|
| 0.137 W/m-K @Temperature 316 °C |
0.951 BTU-in/hr-ft²-°F @Temperature 601 °F |
||
| 0.145 W/m-K @Temperature 500 °C |
1.01 BTU-in/hr-ft²-°F @Temperature 932 °F |
||
| 0.172 W/m-K @Temperature 700 °C |
1.19 BTU-in/hr-ft²-°F @Temperature 1290 °F |
||
| Melting Point | 1800 °C | 3270 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.568 | 1.568 |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 62.5 % | 62.5 % | |
| B2O3 | 13 % | 13 % | |
| SiO2 | 24.5 % | 24.5 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 5.2 @Frequency 9.375e+9 Hz |
5.2 @Frequency 9.375e+9 Hz |
|
| Dissipation Factor | 0.018 @Frequency 9.375e+9 Hz |
0.018 @Frequency 9.375e+9 Hz |