AIM 70 Fusible Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer AIM Specialty Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AIM 70 Fusible Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Uses: punch and die in short run sheet metal forming; external and internal support for bending tubing extrusions; holding jet engine blades for machining and broaching; annealing and nitriding seals; nests for feeding stations.These silvery white alloys expand only ~3.3% of their volume when changing from liquid to solid form, which makes these alloys ideal for many industrial applications. AIM fusible alloys are rarely consumed in an operation and therefore can be remelted and used multiple times. These alloys are normally used in gravity casting but also can be used in other casting methods.Information provided by AIM Specialty Materials.
Physical Properties Metric English Comments
Density 9.38 g/cc
0.339 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 9.2
9.2
Tensile Strength, Ultimate 41.3 MPa
5990 psi
Elongation at Break 200 %
200 %
Thermal Properties Metric English Comments
Heat of Fusion 32.6 J/g
14.0 BTU/lb
CTE, linear 22.0 µm/m-°C

@Temperature 20.0 °C
12.2 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.167 J/g-°C
0.0400 BTU/lb-°F
Liquid
0.167 J/g-°C
0.0400 BTU/lb-°F
Solid
Melting Point 158 °C
316 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 50 %
50 %
Cadmium, Cd 10 %
10 %
Lead, Pb 26.7 %
26.7 %
Tin, Sn 13.3 %
13.3 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000430 ohm-cm
0.0000430 ohm-cm