ATI Allvac® Nickelvac® TJA-1537™ UNS R31537 & UNS R31538 Nickel Superalloy

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® TJA-1537™ UNS R31537 & UNS R31538 Nickel Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Cobalt-base alloy for machined and forged medical and surgical devices requiring high fatigue strength; total joint replacement.Property values are for samples in the metallurgical condition: Warm worked.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 8.30 g/cc
0.300 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 41
41
Tensile Strength, Ultimate 1311 MPa
190100 psi
Tensile Strength, Yield 966 MPa
140000 psi
0.2% Offset
Elongation at Break 20 %
20 %
Reduction of Area 20 %
20 %
Component Elements Properties Metric English Comments
Carbon, C 0.060 %
0.060 %
Chromium, Cr 28 %
28 %
Cobalt, Co 64 %
64 %
as balance
Iron, Fe 0.25 %
0.25 %
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 6.0 %
6.0 %
Nickel, Ni 0.20 %
0.20 %
Nitrogen, N 0.20 %
0.20 %
Silicon, Si 0.50 %
0.50 %