Aclo Accucomp ABS ABS804L High Impact Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Aclo Compounders
Trade Name Accucomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accucomp ABS ABS804L High Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
MD; ASTM D955
Melt Flow 0.40 g/10 min
0.40 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 1.40 GPa
203 ksi
ASTM D638
Flexural Strength 53.0 MPa
7690 psi
ASTM D790
Flexural Modulus 1.900 GPa
275.5 ksi
ASTM D790
Izod Impact, Notched 4.70 J/cm
8.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.9 °C
183 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
163 °F