| Category | Polymer , Thermoplastic , Fluoropolymer , PTFE |
| Manufacturer | Adamas |
| Trade Name | Adalon® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adamas Adalon® 911 PTFE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.12 - 2.20 g/cc | 2.12 - 2.20 g/cc | ASTM D792 |
| Deformation | 10 - 12.9 % | 10 - 12.9 % | ASTM D621 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 54 - 57 | 54 - 57 | ASTM D2240 |
| Ball Indentation Hardness | >= 22.0 MPa | >= 3190 psi | ISO 2032-N132 |
| Tensile Strength at Break | >= 23.0 MPa | >= 3340 psi | ASTM D4745-11 |
| Elongation at Break | >= 260 % | >= 260 % | ASTM D4745-11 |
| Tensile Modulus | >= 0.600 GPa | >= 87.0 ksi | DIN 53457 |
| Coefficient of Friction, Dynamic | 0.060 - 0.080 | 0.060 - 0.080 | ASTM D1894 |
| Coefficient of Friction, Static | 0.080 - 0.11 | 0.080 - 0.11 | ASTM D1894 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C 177 |
| Melting Point | 327 °C | 621 °F | DSC |
| Maximum Service Temperature, Air | 260 °C | 500 °F | DSC |
| Minimum Service Temperature, Air | -200 °C | -328 °F | DSC |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Dielectric Constant | 2.1 @Frequency 60.0 - 2.00e+6 Hz |
2.1 @Frequency 60.0 - 2.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 20.0 - 70.0 kV/mm | 508 - 1780 kV/in | ASTM D149 |