| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Talc Filler |
| Manufacturer | Adell Plastics, Inc. |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Adell EA-18 Homopolymer Polypropylene, 40% Talc Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.235 g/cc | 0.04462 lb/in³ | ASTM D792 |
| Water Absorption | 0.040 % | 0.040 % | 24 hour immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0080 cm/cm | 0.0080 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 70 | 70 | ASTM D785 |
| Hardness, Rockwell R | 101 | 101 | ASTM D785 |
| Tensile Strength, Ultimate | 31.7 MPa | 4600 psi | ASTM D638 |
| Elongation at Break | 10 % | 10 % | ASTM D638 |
| Flexural Strength | 51.0 MPa | 7400 psi | ASTM D790 |
| Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
| Izod Impact, Notched | 0.200 J/cm | 0.375 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 2.30 J/cm | 4.31 ft-lb/in | ASTM D256 |
| Gardner Impact | 0.600 J | 0.443 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 182 °C | 360 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 132 °C | 270 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |