Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Applied Composites 8061 Polyester SMC

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Applied Composites Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Composites 8061 Polyester SMC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Structural Grade Chopped Fibers, High Stiffness, High Fiber LoadingsInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 55
55
ASTM D2583
Tensile Strength, Ultimate 172 MPa
25000 psi
ASTM D638
Tensile Modulus 17.2 GPa
2500 ksi
ASTM D638
Flexural Strength 365 MPa
53000 psi
ASTM D790
Flexural Modulus 14.5 GPa
2100 ksi
Tangent; ASTM D790
Izod Impact, Notched 10.7 J/cm
20.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
Flexural Load; ASTM D648
Users viewing this material also viewed the following: