| Category | Ceramic , Oxide , Silicon Oxide , Zirconium Oxide |
| Manufacturer | Aremco |
| Trade Name | Ceramacast™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | 1.56 g/cc | 0.0562 lb/in³ | Powder |
| Porosity | <= 5.0 % | <= 5.0 % | |
| pH | 5.0 - 6.0 | 5.0 - 6.0 | |
| Viscosity | 25000 cP | 25000 cP |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Compressive Strength | 55.2 MPa | 8000 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 5.04 µm/m-°C @Temperature 20.0 °C |
2.80 µin/in-°F @Temperature 68.0 °F |
|
| Maximum Service Temperature, Air | 1540 °C | 2800 °F | |
| Shrinkage | <= 1.00 % @Temperature 538 °C |
<= 1.00 % @Temperature 1000 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm | |
| Dielectric Strength | 4.92 kV/mm | 125 kV/in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Dry Time | >= 8 hour | >= 8 hour | Air dry |
| Cure Time | 300 - 420 min | 5.00 - 7.00 hour | 2-4 hrs at 200°F; 3 hrs at 250°F |
| Pot Life | <= 20 min | <= 20 min | |
| Shelf Life | 12.0 Month | 12.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Acid Resistance | Good | |
| Alkali Resistance | Good | |
| Color | Off White | |
| Mix Ratio | 100:15-17 | |
| Moisture Resistance | Good |