Material Notes:
OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between PEX, PE, PA, and EVOH. It is combined with SOARNOL from NIPPON GOSHEI provides very good oxygen barrier. These tubes are used in plumbing, sanitary, heating floor and also industrial applications.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.916 g/cc

@Temperature 23.0 °C
0.0331 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Index of Compound 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ISO 868
Tensile Strength at Break 24.0 MPa
3480 psi
ASTM D638
Tensile Strength, Yield 6.50 MPa
943 psi
ASTM D638
Elongation at Break 930 %
930 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 121 °C
250 °F
DSC
Vicat Softening Point 92.0 °C

@Load 0.999 kg
198 °F

@Load 2.20 lb
ISO 306
Processing Properties Metric English Comments
Zone 1 160 - 180 °C
320 - 356 °F
Zone 2 180 - 200 °C
356 - 392 °F
Zone 3 200 - 220 °C
392 - 428 °F
Zone 4 210 - 230 °C
410 - 446 °F
Die Temperature 220 - 240 °C
428 - 464 °F