| Category | Polymer , Thermoplastic , Nylon |
| Manufacturer | Arkema |
| Trade Name | Orgalloy® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Arkema Group Orgalloy® LT 6040IH Nylon (Conditioned).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.10 g/cc | 0.0397 lb/in³ | |
| Melt Flow | 1.5 g/10 min @Load 5.00 kg, Temperature 235 °C |
1.5 g/10 min @Load 11.0 lb, Temperature 455 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 28.0 MPa | 4060 psi | 50 mm/min |
| Elongation at Break | >= 50 % | >= 50 % | Nominal Strain; 50 mm/min |
| Elongation at Yield | 9.0 % | 9.0 % | 50 mm/min |
| Tensile Modulus | 0.650 GPa | 94.3 ksi | 1 mm/min |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 20.0 °C |
94.4 µin/in-°F @Temperature 68.0 °F |
|
| CTE, linear, Transverse to Flow | 177 µm/m-°C @Temperature 20.0 °C |
98.3 µin/in-°F @Temperature 68.0 °F |
|
| Melting Point | 220 °C | 428 °F | 10°C/min |
| Flammability, UL94 | V-2 @Thickness 1.60 mm |
V-2 @Thickness 0.0630 in |
|
| V-0 @Thickness 3.20 mm |
V-0 @Thickness 0.126 in |
||
| Oxygen Index | 29 % | 29 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 600 V | 600 V |