Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® Clear 400 Polyether Block Amide (PEBA)

Category Polymer , Thermoplastic , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Pebax® Clear 400 Polyether Block Amide (PEBA).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Pebax® Clear 400 combines high transparency level with the unique performance of Pebax®, thermoplastic elastomer made of flexible polyether and rigid polyamide.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
Instantaneous, Conditioned 15 days at 23°C - 50% RH; ISO 868
56

@Time 15.0 sec
56

@Time 0.00417 hour
Conditioned 15 days at 23°C - 50% RH; ISO 868
Tensile Strength at Break 54.0 MPa
7830 psi
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Elongation at Break >= 350 %
>= 350 %
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Flexural Modulus 0.340 GPa
49.3 ksi
Conditioned 15 days at 23°C - 50% RH; ISO178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Melting Point 159 °C
318 °F
ISO 11357
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Nozzle Temperature 240 °C
464 °F
Recommended
210 - 270 °C
410 - 518 °F
Mold Temperature <= 30.0 °C
<= 86.0 °F
Surface: Mirror polish to get the optimum transparency
Drying Temperature 60.0 °C
140 °F
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Users viewing this material also viewed the following: