Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Dry)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Water Absorption 1.2 %
1.2 %
Moisture Absorption at Equilibrium 0.50 %
0.50 %
Humidity Absorption
Melt Flow 9.0 g/10 min

@Load 1.00 kg,
Temperature 235 °C
9.0 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
Tensile Strength, Yield 6.20 MPa

@Strain 50.0 %
899 psi

@Strain 50.0 %
50 mm/min
Tensile Modulus 0.0510 GPa
7.40 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched NB
NB
1.27 J/cm²

@Temperature -30.0 °C
6.04 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
10°C/min
Glass Transition Temp, Tg -65.0 °C
-85.0 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in
Electrical Properties Metric English Comments
Electrical Resistivity 4.44e+13 ohm-cm
4.44e+13 ohm-cm
Surface Resistance 1.69e+13 ohm
1.69e+13 ohm
Dielectric Strength 43.0 kV/mm
1090 kV/in
Dissipation Factor 0.00051

@Frequency 1e+6 Hz
0.00051

@Frequency 1e+6 Hz
0.00081

@Frequency 100 Hz
0.00081

@Frequency 100 Hz
Users viewing this material also viewed the following: