Material Notes:
A reinforced, flame retardant resin with outstanding structural strength. Good appearance and high impact.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 68.0 MPa
9860 psi
ATSM D638
Flexural Strength 106 MPa
15400 psi
ASTM D790
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Izod Impact, Notched 1.55 J/cm
2.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648