Axiall 21540 Coax & Telecom Flexible PVC Black 307

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 21540 Coax & Telecom Flexible PVC Black 307.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation. Max service temperature rating of 80°C at 0.006" wall. This product contains 2% of a 20nm carbon black.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.34 g/cc
1.30 - 1.34 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 52 - 58
52 - 58
delayed; ASTM D-2240
Tensile Strength, Yield 22.8 MPa
3300 psi
ASTM D-638
Elongation at Yield 253.8 %
253.8 %
Air Aging: 7 days @ 121°C; 30 mil slabs; UL 1581
300 %
300 %
ASTM D-638
100% Modulus 0.0190 GPa
2.75 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 32 %
32 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
50% RH; ASTM D-257
Dielectric Constant 2.56

@Frequency 1e+6 Hz
2.56

@Frequency 1e+6 Hz
3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F