Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Elastollan C 59 D TPUR

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer BASF
Trade Name Elastollan
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Elastollan C 59 D TPUR.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilience performance.Typical Applications: Spiral tubing, pneumatic tubing, round and v-belting, technical moldings, e.g. bushes, dust caps, seals, blow molding bellows, and mining screens.Note: Quoted results are from measurements on injection molded test platens, post tempered for 20 hours at 100°CInformation provided by BASF
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183-1-A
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ISO 686
Tensile Strength 43.0 MPa
6240 psi
after storage in water at 80°C for 42 days; ISO 37
50.0 MPa
7250 psi
ISO 37
12.0 MPa

@Strain 20.0 %
1740 psi

@Strain 20.0 %
ISO 37
17.0 MPa

@Strain 100 %
2470 psi

@Strain 100 %
ISO 37
30.0 MPa

@Strain 300 %
4350 psi

@Strain 300 %
ISO 37
Elongation at Break 480 %
480 %
after storage in water at 80°C for 42 days; ISO 37
500 %
500 %
ISO 37
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
DIN EN ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
DIN EN ISO 179
Tear Strength 160 kN/m
913 pli
DIN ISO 34-1/Bb
Abrasion 20
20
[mm<sup>3</sup>; ISO 4649
Compression Set 30 %

@Temperature 23.0 °C
30 %

@Temperature 73.4 °F
ISO 815
50 %

@Temperature 70.0 °C
50 %

@Temperature 158 °F
ISO 815
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Processing Temperature 170 - 240 °C
338 - 464 °F
Injection molding
Mold Temperature 20.0 - 70.0 °C
68.0 - 158 °F
Descriptive Properties Value Comments
Commercial Status North America
Primary Processing Technique Injection molding
Copyright © lookpolymers.com All Rights Reserved