| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled , Polyethylene Terephthalate (PET) |
| Manufacturer | BASF |
| Trade Name | Ultradur B |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | BASF Ultradur B 4040 G6 LS High Speed BK15029 30% Glass Filled PBT/PET.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.56 g/cc | 0.0564 lb/in³ | ISO 1183 |
| Viscosity Test | 87 cm³/g | 87 cm³/g | Viscosity number |
| Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 275 °C |
50 g/10 min @Load 4.76 lb, Temperature 527 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 135 MPa | 19600 psi | 5mm/min; ISO 527 |
| Elongation at Break | 1.8 % | 1.8 % | 5mm/min; ISO 527 |
| Tensile Modulus | 10.7 GPa | 1550 ksi | 1mm/min; ISO 527 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 232 °C | 450 °F | 10 K/min |
| Deflection Temperature at 0.46 MPa (66 psi) | 215 °C | 419 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | ISO 75 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | BK15029 | |
| Commercial Status | Active America | |
| Impact Modified | No | |
| Primary Processing Technique | Injection Molding |