BASF Ultrason® E 2020 P SR PESU

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer BASF
Trade Name Ultrason®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultrason® E 2020 P SR PESU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Polyethersulfone flakes, e.g. for membrane applications, coatings and resin modification, containing min. 50% of OH-endgroups. The product is soluble in N-methyl-pyrrolidone (NMP) and N,N-Dimethylacetamide (DMAc). This type is not suitable for injection molding. Abbreviated designation according to ISO 1043-1: PESUInformation provided by BASF
Physical Properties Metric English Comments
Bulk Density 0.250 - 0.300 g/cc
0.00903 - 0.0108 lb/in³
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.0 %
1.0 %
23°C; 50% RH; ISO 62
Viscosity Measurement 59
59
[cm<sup>3</sup>/g]; ISO 307
Mechanical Properties Metric English Comments
Tensile Modulus 2.70 GPa
392 ksi
ISO 527-1/-2
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 225 °C
437 °F
ISO 11357-1/-2
Decomposition Temperature >= 400 °C
>= 752 °F
Processing Properties Metric English Comments
Drying Temperature 140 °C
284 °F
Dry Time 4 hour
4 hour
Descriptive Properties Value Comments
Ignition Temperature 580-600°C
DIN 54836