| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Fiber Filled, Flame Retardant |
| Manufacturer | Beijing Chemical Industry Research Institute (Group) |
| Trade Name | KAIFA® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Beijing Chemical Industry KAIFA® MN301-G35 Nylon 66 Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 125 MPa | 18100 psi | ASTM D638 |
| Flexural Strength | 215 MPa | 31200 psi | ASTM D790 |
| Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO179 |
| Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | ASTM D648 |
| Flammability, UL94 | V-0 @Thickness 3.20 mm |
V-0 @Thickness 0.126 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.2 @Frequency 1e+6 Hz |
3.2 @Frequency 1e+6 Hz |
ASTM D150 |
| Dielectric Strength | 30.0 kV/mm @Thickness 2.00 mm |
762 kV/in @Thickness 0.0787 in |
ASTM D149 |
| Dissipation Factor | 0.018 @Frequency 1e+6 Hz |
0.018 @Frequency 1e+6 Hz |
ASTM D150 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
| Middle Barrel Temperature | 265 - 270 °C | 509 - 518 °F | |
| Front Barrel Temperature | 265 - 270 °C | 509 - 518 °F | |
| Nozzle Temperature | 265 - 270 °C | 509 - 518 °F | |
| Mold Temperature | 60.0 - 90.0 °C | 140 - 194 °F | |
| Drying Temperature | 130 °C | 266 °F | |
| Dry Time | 4 hour | 4 hour | |
| Injection Pressure | 90.0 - 120 MPa | 13100 - 17400 psi |