Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis FR4847 Polyethylene Based Striping Compound

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis FR4847 Polyethylene Based Striping Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FR4847 is a Polyethylene Based Striping Compound for Primary Automotive Wires. FR4847 is designed and manufactured with advanced material and processing technology to provide enhanced stabilization and lower particulate matter. This compound was designed to have high compatibility with our chemically crosslinkable non-halogen flame retardant insulation compounds. Application: FR4847 is intended for use as non-halogen flame retardant polyethylene compound in striping applications for primary automotive wires. It would be used in conjunction with our chemically crosslinkable nonhalogen flame retardant insulation compounds.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 48
48
ASTM D2240
Tensile Strength at Break 9.00 MPa
1310 psi
ASTM D412
Elongation at Break 280 %
280 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Dielectric Constant 3.7

@Frequency 6.00e+7 Hz
3.7

@Frequency 6.00e+7 Hz
ASTM D150
Dielectric Strength >= 22.0 kV/mm
>= 559 kV/in
Dissipation Factor 0.010

@Frequency 6.00e+7 Hz
0.010

@Frequency 6.00e+7 Hz
ASTM D150
Processing Properties Metric English Comments
Processing Temperature 55.0 °C
131 °F
drying;2-8h
Middle Barrel Temperature 121 °C
250 °F
Melt Temperature 120 - 125 °C
248 - 257 °F
Shelf Life 12.0 Month
12.0 Month
Users viewing this material also viewed the following: