Material Notes:
H 125 is a high melt flow rate homopolymer designed for nonwoven by spunbonded processing. It is used in fiber extrusion processing. This resin features excellent processing, allowing increased line speed or air pressure, as well as gains on mechanical properties. The narrow molecular weight distribution, special stability, and tight gel appearance control provide its unique performance. Its applications include: high-performance spunbond nonwovens for hygiene disposables and hospital products; nonwovens for furniture and decoration; and low-title and/or high-speed spinning multifilaments.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 38 g/10 min

@Load 2.16 kg,
Temperature 230 °C
38 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM-D785
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM-D638
Elongation at Yield 13 %
13 %
ASTM-D638
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM-D790
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM-D648
Vicat Softening Point 154 °C

@Load 1.02 kg
309 °F

@Load 2.25 lb