A 40% mineral reinforced nylon 66 exhibiting excellent stiffness in parts where control of warpage is essential.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 90.0 MPa
13100 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 6.60 GPa
957 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 288 °C
550 °F