| Category | Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified |
| Manufacturer | Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong) |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Cheng Yu Plastic IPS600 Flame Retardant HIPS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
| Melt Index of Compound | 8.0 - 10 g/10 min | 8.0 - 10 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 102 | 102 | ASTM D785 |
| Tensile Strength, Yield | 37.4 MPa | 5420 psi | ASTM D638 |
| Flexural Yield Strength | 63.7 MPa | 9250 psi | ASTM D790 |
| Izod Impact, Notched | 0.834 J/cm | 1.56 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 80.0 °C | 176 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 |