| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, PTFE Filled |
| Manufacturer | Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong) |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Cheng Yu Plastic ML1010 PC/PTFE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.26 g/cc | 1.26 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 82 | 82 | ASTM D785 |
| Tensile Strength, Yield | 53.9 MPa | 7820 psi | ASTM D638 |
| Flexural Yield Strength | 68.6 MPa | 9960 psi | ASTM D790 |
| Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 136 °C | 277 °F | ASTM D648 |
| Flammability, UL94 | V-2 | V-2 |