| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Glass + PTFE Filled |
| Manufacturer | Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong) |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Cheng Yu Plastic ML1210 PC/PTFE, 10% Glass.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.34 g/cc | 1.34 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 90 | 90 | ASTM D785 |
| Tensile Strength, Yield | 1.47 MPa | 213 psi | ASTM D638 |
| Flexural Yield Strength | 83.36 MPa | 12090 psi | ASTM D790 |
| Izod Impact, Notched | 10.6 J/cm | 19.8 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 149 °C | 300 °F | ASTM D648 |
| Flammability, UL94 | V-2 | V-2 |