Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips K-Resin® BK13 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips K-Resin® BK13 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Styrene-Butadiene CopolymerBK13 is an SBC developed specifically to have enhanced flow capabilities and improved stiffness over the KR01 grade. BK13 molded parts give excellent detail on rapid production cycles, and are easily processed by injection molding. This resin can be tinted or colored in a variety of transparent and opaque shades.Applications: Major applications include displays, medical devices, overcaps, housings, and toys.Processing Recommendations:Injection Molding: Minimum melt temperature between 193-232°C necessary to permit mold fill. Minimum injection pressure required to fill the cavity. Maximum back pressure of 0.3 MPa. Drying: Generally, no need to dry resin.Specification Data: FDA Regulation 21 CFR 177.1640; suitable for food contact. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50.Data provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 200 °C
15 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ASTM D2240
Tensile Strength, Yield 39.0 MPa
5660 psi
2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Elongation at Break 5.0 %
5.0 %
2 in per min; ASTM D638; Test specimens were injection molded by ASTM D1897.
Flexural Yield Strength 69.0 MPa
10000 psi
Test specimens were injection molded by ASTM D1897; ASTM D790
Flexural Modulus 2.158 GPa
313.0 ksi
Test specimens were injection molded by ASTM D1897; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
ASTM D648
Vicat Softening Point 89.0 °C
192 °F
ASTM D1525
Optical Properties Metric English Comments
Transmission, Visible 93 %
93 %
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 193 - 232 °C
379 - 450 °F
Injection
Users viewing this material also viewed the following: