Material Notes:
Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
Mechanical Properties Metric English Comments
Tensile Strength 30.411 MPa
4410.8 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 68.67 MPa
9960 psi
ASTM D790
Flexural Modulus 2.7468 GPa
398.39 ksi
ASTM D790
Izod Impact, Notched 0.412 J/cm
0.771 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 133 °C
271 °F
ASTM D648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Melt Temperature 170 - 200 °C
338 - 392 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F