| Category | Polymer , Thermoplastic , Polyester, TP |
| Manufacturer | Eastman Chemical |
| Trade Name | Ecdel |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eastman Ecdel PCCE 9967 Copolyester Ether Elastomer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Elongation at Break | >= 50 % | >= 50 % | |
| Tensile Modulus | 0.132 GPa | 19.1 ksi | 1mm/min |
| Charpy Impact Unnotched | NB | NB | |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
||
| Charpy Impact, Notched | NB | NB | |
| 0.820 J/cm² @Temperature -30.0 °C |
3.90 ft-lb/in² @Temperature -22.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 189 µm/m-°C @Temperature 20.0 °C |
105 µin/in-°F @Temperature 68.0 °F |
|
| CTE, linear, Transverse to Flow | 184 µm/m-°C @Temperature 20.0 °C |
102 µin/in-°F @Temperature 68.0 °F |
|
| Melting Point | 199 °C | 390 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 63.0 °C | 145 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 46.0 °C | 115 °F | |
| Vicat Softening Point | 53.0 °C | 127 °F | |
| Glass Transition Temp, Tg | -3.00 °C | 26.6 °F |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 225 - 260 °C | 437 - 500 °F |