| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
| Melt Flow | 0.40 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.40 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
| 0.80 g/10 min @Load 3.80 kg, Temperature 230 °C |
0.80 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 100 | 100 | ASTM D785 |
| Tensile Strength, Yield | 34.5 MPa | 5000 psi | ASTM D638 |
| Elongation at Break | 40 % | 40 % | ASTM D638 |
| Tensile Modulus | 2.31 GPa | 335 ksi | ASTM D638 |
| Flexural Yield Strength | 55.2 MPa | 8000 psi | ASTM D790 |
| Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
| Izod Impact, Notched | 3.84 J/cm | 7.20 ft-lb/in | 0.125 in; ASTM D256 |
| 4.32 J/cm | 8.10 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 119 µm/m-°C @Temperature -40.0 - 176 °C |
66.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C | 205 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 86.1 °C | 187 °F | Unannealed; ASTM D648 |
| Vicat Softening Point | 106 °C | 223 °F | ASTM D1525 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 191 - 210 °C | 375 - 410 °F | |
| Zone 2 | 191 - 210 °C | 375 - 410 °F | |
| Zone 3 | 199 - 221 °C | 390 - 430 °F | |
| Zone 4 | 199 - 221 °C | 390 - 430 °F | |
| Zone 5 | 199 - 221 °C | 390 - 430 °F | |
| Adapter Temperature | 221 - 241 °C | 430 - 465 °F | |
| Die Temperature | 221 - 241 °C | 430 - 465 °F | |
| Drying Temperature | 85.0 °C | 185 °F | |
| Dry Time | 3 hour | 3 hour | |
| Moisture Content | <= 0.020 % | <= 0.020 % |