Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil 100 Mobil Aviation Grease SHC

Category Fluid , Lubricant , Lithium Gellant , Polyalphaolefin (PAO)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil 100 Mobil Aviation Grease SHC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Mobil Aviation Grease SHC 100 is a supreme performance synthetic grease which combines the unique features of a polyalphaolefin (PAO) synthetic base fluid with those of a high quality lithium complex soap thickener.  The thickener system provides a high dropping point, excellent resistance to water wash, and a tenacious structural stability.  The unique physical properties of the synthetic base oil, combined with selected additives, provide outstanding protection against wear, rust, corrosion, and high temperature degradation.  The wax-free feature of the synthetic base oil allows for low-temperature mobility/pumpability and low starting and running torque values.  Also, the traction property of the synthetic base fluid is considerably lower than mineral, allowing for temperature reductions in the load zone of rolling element bearings.  Mobil Aviation Grease SHC 100 is the product of choice for aircraft wheel bearing applications.Mobil Aviation Grease SHC 100 is recommended for aviation applications which need a lubricant that can perform normal functions, yet go far beyond in terms of high and low temperatures and long-life performance.  It is a NLGI Grade 2/ISO VG 100 grease having the cold-temperature pumping resistance of most mineral-oil NLGI Grade 0 greases.  It provides outstanding protection at operating temperatures from –54 ºC (-65 ºF) to 177 ºC (350 ºF). Mobil Aviation grease SHC 100 is recommended for high speed, heavy load applications such as wheel bearings, as well as for slower speed, high load applications such as landing gear bearings, slides, and joints. Mobil Aviation Grease SHC 100 is approved as a wheel bearing grease by all major aircraft wheel manufacturers.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 100 cSt
100 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 14.5 cSt
14.5 cSt
ASTM D445
Oxidative Stability 100 hour
100 hour
Pressure Drop of 3 kPa; ASTM D942
500 hour
500 hour
Pressure Drop of 5 kPa; ASTM D942
Evaporation Loss 5.0 %
5.0 %
30 hrs @ 177°C; ASTM D972
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 40
40
ASTM D2596
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
Four Ball Wear 0.300 mm
0.0118 in
ASTM D2266
Penetration 280
280
60 Stroke Worked @ 25°C, mm/10; ASTM D217
305
305
Extended Worked Penetration Stability, 100000 Strokes, mm/10; FTM 313
Oil Separation 8.0 %
8.0 %
30 hrs @ 177°C; ASTM D6184
Thermal Properties Metric English Comments
Dropping Point 278 °C
532 °F
ASTM D2265
Descriptive Properties Value Comments
Color red
Copper Strip Corrosion, ASTM D4048 1B (max)
Corrosion Prevention, ASTM D1743 pass
48 hrs @ 125°F
Particle Count, 25-50 microns pass, 25-125 microns, dirt count, particles/mL, FTM 3005, pass 125 micron or larger
Soap/Thickener Type lithium complex
Structure smooth; slight tack
Water Washout, ASTM D1264, wt% 3
1 hr @ 41°C
7
1hr @ 79°C
Users viewing this material also viewed the following: