Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 8203-45 Thermoplastic Rubber  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8203-45 Thermoplastic Rubber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: A colorable thermoplastic general purpose non-hygroscopic elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be processed using injection molding, extrusion, blow molding or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags.Features: Non-hygroscopic product, requires little to no drying before processingNeutral, easy coloring formulationExcellent ozone resistanceexcellent flex fatigue resistanceSuperb surface appearance and minimal flow imperfectionsProduct Notes: Values are for injection molded plaques, side gated.102.6 mm x 152 mm x 2 mmInformation provided by Advanced Elastomer Systems.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
15 seconds; ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
Across flow; ASTM D412
Tensile Strength, Yield 11.0 MPa

@Strain 100 %
1600 psi

@Strain 100 %
across flow; ASTM D412
Elongation at Break 770 %
770 %
Across flow; ASTM D412
Processing Properties Metric English Comments
Processing Temperature 177 - 232 °C
351 - 450 °F
Drying Temperature 82.0 °C
180 °F
Desiccant Dryer
Dry Time 3 hour
3 hour
Desiccant Dryer