Fainplast Compounds RKS 321 Rigid PVC, Antishock Extrusion Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds RKS 321 Rigid PVC, Antishock Extrusion Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Outdoor antishock profiles
Physical Properties Metric English Comments
Density 1.42 - 1.46 g/cc
0.0513 - 0.0527 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.0 MPa
5660 psi
ISO R 527
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO R527
Elongation at Break 130 %
130 %
ISO R 527
Izod Impact, Unnotched 9.80 - 10.2 J/cm

@Temperature 23.0 °C
18.4 - 19.1 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 84.0 - 86.0 °C

@Load 5.00 kg
183 - 187 °F

@Load 11.0 lb
ISO R306