Glass Type: Bi-Pb-Zn Typical Powder Form: MVG Typical Application: End Termination Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conductors, end terminations, over glazes, and dielectrics.Information provided by Ferro Corporation
Physical Properties Metric English Comments
Density 7.57 g/cc
0.273 lb/in³
Particle Size 5.0 µm
5.0 µm
50% of particles
<= 25 µm
<= 25 µm
Thermal Properties Metric English Comments
CTE, linear 11.6 µm/m-°C
6.44 µin/in-°F
at Set Pt.
10.8 µm/m-°C

@Temperature 260 °C
6.00 µin/in-°F

@Temperature 500 °F
Softening Point 434 °C
813 °F
Annealing Point 360 °C
680 °F
Transformation Temperature 345 °C
653 °F
Processing Properties Metric English Comments
Processing Temperature 600 °C
1110 °F
Typical Firing Temperature