Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Global PC/ABS-1211 General Purpose Polycarbonate/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Global Polymers Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global PC/ABS-1211 General Purpose Polycarbonate/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Global Polymers Corporation.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
11 g/10 min

@Load 3.80 kg,
Temperature 230 °C
11 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ASTM D638
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM D256
Users viewing this material also viewed the following: