H.C. Starck Glass Melting Electrodes made from Electron Beam Melted Molybdenum

Category Metal , Nonferrous Metal , Molybdenum Alloy , Refractory Metal
Manufacturer H.C. Starck
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Glass Melting Electrodes made from Electron Beam Melted Molybdenum.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description of Product: The electrodes are manufactured by electron beam melting from pure molybdenum and are supplied to customer requirements by forging or machining.Range of Application: Electron beam melted molybdenum is preferentially used for the production of glass melting electrodes (GME).Structure: the material can be offered as forged as well as recrystallized (after annealing).Information provided by H.C. Starck.
Physical Properties Metric English Comments
Density >= 10.2 g/cc
>= 0.368 lb/in³
Component Elements Properties Metric English Comments
Carbon, C <= 0.0030 %
<= 0.0030 %
Chromium, Cr <= 0.0010 %
<= 0.0010 %
Cobalt, Co <= 0.0015 %
<= 0.0015 %
Copper, Cu <= 0.0010 %
<= 0.0010 %
Iron, Fe <= 0.0040 %
<= 0.0040 %
Lead, Pb <= 0.0010 %
<= 0.0010 %
Manganese, Mn <= 0.0010 %
<= 0.0010 %
Molybdenum, Mo >= 99.95 %
>= 99.95 %
Balance
Nickel, Ni <= 0.0015 %
<= 0.0015 %
Oxygen, O <= 0.0030 %
<= 0.0030 %
Tungsten, W >= 0.030 %
>= 0.030 %
Zinc, Zn <= 0.0010 %
<= 0.0010 %