Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® M32 Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M32 Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HexPly® M32 is specifically designed for prepreg applications with fabrics and short curing cycles for sporting (e.g. ski and snowboard production) and industrial applications. HexPly® M32 comprises a modified epoxy resin preimpregnated into carbon, glass or aramid fibers. A typical curing cycle would be 9 min at 120ºC.Features: Suited to press and autoclave manufacturing methods, Short curing cycle at 110-130ºC, Good drapability, Medium to low tack, Suitable for a range of pressure cycles (1-10 bar), Controlled flow for ease of processing, Excellent adhesive properties, Tough epoxy matrix
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 100 °C
212 °F
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature -18.0 °C
6.00 Month

@Temperature -0.400 °F