Material Notes:
RenShape® SL 7820 stereolithography material is a white, low viscosity and stable liquid that produces strong black models and prototypes with good surface fi nish and detail, and ABS-like appearance. It offers a large working envelope of physical properties, high elongation and impact strength suitable for building concept models, and functional prototype parts. Information provided by Huntsman.
Physical Properties Metric English Comments
Density 1.13 g/cc

@Temperature 25.0 °C
0.0408 lb/in³

@Temperature 77.0 °F
Liquid
1.16 g/cc

@Temperature 25.0 °C
0.0419 lb/in³

@Temperature 77.0 °F
Solid
Viscosity 210 cP

@Temperature 30.0 °C
210 cP

@Temperature 86.0 °F
240 cP

@Temperature 28.0 °C
240 cP

@Temperature 82.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Tensile Strength 36.0 - 51.0 MPa
5220 - 7400 psi
ASTM D638
Elongation at Break 8 - 18 %
8 - 18 %
ASTM D638
Tensile Modulus 1.90 - 2.40 GPa
276 - 348 ksi
ASTM D638
Flexural Strength 59.0 - 80.0 MPa
8560 - 11600 psi
ASTM D790
Flexural Modulus 2.00 - 2.40 GPa
290 - 348 ksi
ASTM D790
Izod Impact, Notched 0.420 - 0.480 J/cm
0.787 - 0.899 ft-lb/in
ASTM D256
Penetration 4.5
4.5
mils penetration depth
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
below Tg; ASTM D648
Glass Transition Temp, Tg 62.0 °C
144 °F
DMA, E"
Descriptive Properties Value Comments
Appearance Dark brown to black
cured
White
liquid
Critical Exposure (Ec) 10 mJ/cm²