Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Devcon
Trade Name Composite Welder™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by ITW Devcon
Physical Properties Metric English Comments
Viscosity 120000 cP
120000 cP
Mixed Viscosity (Thixotropic gel)
Mechanical Properties Metric English Comments
Elongation at Break 100 - 125 %
100 - 125 %
Adhesive Bond Strength 15.5 MPa
2250 psi
lap shear (on grit blasted steel, bond line thickness of 0.010"); ASTM D1002
Tensile Impact Strength 46.2 kJ/m²
22.0 ft-lb/in²
Peel Strength 10.5 - 11.4 kN/m
60.0 - 65.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
dry
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
dry
Processing Properties Metric English Comments
Cure Time 4.00 - 8.00 min
0.0667 - 0.133 hour
Working time
10.0 - 15.0 min
0.167 - 0.250 hour
Fixture time
45.0 - 60.0 min
0.750 - 1.00 hour
Functional cure
Descriptive Properties Value Comments
Mix ratio (Resin:Hardener) 10:1