| Category | Ceramic , Clay , Kaolin Clay , Oxide , Aluminum Oxide , Silicon Oxide |
| Manufacturer | Imerys (Kentucky-Tennessee Clay Co.) |
| Trade Name | Amlock™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Imerys Amlockâ„¢ 321 Kaolin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.60 g/cc | 2.60 g/cc | |
| Brightness | 70 - 80 % | 70 - 80 % | G.E. Brightness |
| Oil Absorption | 33 - 38 % | 33 - 38 % | g/100g clay; ASTM D-281 |
| Particle Size | 0.20 µm | 0.20 µm | 34% finer than |
| 0.30 µm | 0.30 µm | median | |
| 0.50 µm | 0.50 µm | 72% finer than | |
| 1.0 µm | 1.0 µm | 86% finer than | |
| 2.0 µm | 2.0 µm | 93% finer than | |
| 5.0 µm | 5.0 µm | 97% finer than | |
| 10 µm | 10 µm | 99% finer than | |
| 20 µm | 20 µm | 99% finer than | |
| Particle Mesh Size | 325 Mesh | 325 Mesh | 0.25% retained |
| pH | 7.0 - 8.0 | 7.0 - 8.0 | |
| Specific Surface Area | 22 - 26 m²/g | 22 - 26 m²/g |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 38.1 % | 38.1 % | |
| CaO | 0.020 % | 0.020 % | |
| Fe2O3 | 1.7 % | 1.7 % | |
| K2O | 0.30 % | 0.30 % | |
| Loss on Ignition(%) | 13.6 % @Temperature 950 °C |
13.6 % @Temperature 1740 °F |
|
| P2O5 | 0.10 % | 0.10 % | |
| SiO2 | 45.1 % | 45.1 % | |
| SO3 | 0.50 % | 0.50 % | |
| TiO2 | 1.6 % | 1.6 % | |
| Zinc, Zn | 0.0027 % | 0.0027 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | white |